Problems of Polymer Melt in Metal Powder Injection Molding
Oct 16, 2022
Problems of Polymer Melt in Metal Powder Injection Molding
In the process of metal powder injection molding, due to the lack of knowledge, its performance will be affected during processing. Generally speaking, the basic characteristics are often ignored. At the same time, simply manufacturing a template through a component is a fault. What problems occur in the polymer melt during metal powder injection molding? Now, let's introduce the problems of polymer melt in metal powder injection molding.
Dahong New Materials found that many metal powder injection molding manufacturers introduced that it is often unnecessary to dry the granules in advance, but the excess moisture will generate steam, and melting will lead to voids. Under the effect of molding, the water in some polymer melts will undergo more severe hydrolysis degradation, leading to brittle molding. Therefore, MIM technical experts recommend that desiccants or vacuum dryers should be used consistently for drying materials of hydrolysis sensitive polymers.
The increase of thermal degradation rate of polymer melt will lead to over heating, which will lead to brittle molding. Sizing can stay in the barrel for a long time, consuming polymer stabilizer. Due to the requirements of high pressure, the molding of polymer degradation in metal powder injection molding is difficult to fill, and will fall into the common trap of temperature rise, reducing the viscosity of the melt, and molding is slower.
Therefore, the leading manufacturer in the MIM industry concluded that when the polymer degrades, it seems easier to fill, the viscosity shear of the polymer melt needs more reaction temperature than it, and a faster filling rate is more effective for the filling cavity.
In general, rapid cooling of polymer melt in metal powder injection molding can shorten the cycle and improve the productivity. It is also a simple way to realize precise and complex parts with precise dimensions (such as MIM automobile parts, powder metallurgy micro gears, powder metallurgy small module gears). At least after demoulding for a period of time, the thermoplastic will not be impacted and will be cooled at a fixed speed. The non-uniform cooling rate leads to shrinkage, which leads to inaccurate size or high residual stress. If the mold temperature is low, the gate with small gate size will quickly separate the melt in the mold cavity and free shrinkage. If so, the molding cycle has long been under high pressure.
The above is about the problems of polymer melt in metal powder injection molding. Dahong New Materials hopes to help you by introducing these little knowledge. If you have other questions, please come to consult the technical team of Dahong New Materials!