S40C Lost Wax Investment Casting
S40C lost wax investment casting has high strength and good machinability, medium cold deformation plasticity, and poor weldability. It can be welded after quenching and tempering.
Product Introduction
|
S40C lost wax investment casting |
|||||||
|
Item |
Material |
Production Process |
Sintering Temperature |
Mold |
Custom |
||
|
S40C lost wax investment casting |
S40C |
Molten mold casting |
1380℃ |
To be customized |
Yes |
||
|
Chemical composition |
Mn: 0.50-0.80 Si: 0.17-0.37 C: 0.37-0.44 |
||||||
|
Available Materials |
Carbon steel, alloy steel, aluminum alloy, low -carbon stainless steel, titanium alloy (TI, TC4), copper alloy, high temperature alloy (718, 713) |
||||||
|
Smoothness |
Dimensional accuracy |
Product density |
Appearance treatment |
Appropriate weight |
|||
|
Roughness 1~5μm |
(±0.1%~±0.5%) |
7.8g/CM³ |
According to customer requirements |
3g~4kg) |
|||
S40C is high-quality carbon structural steel
Corresponding brand
National standard grade 40 steel
Japanese brand number S40C
American Standard No. 1040
German brand number 1.1186
Characteristics and scope of application
S40C lost wax investment casting has high strength and good machinability, medium cold deformation plasticity, and poor weldability. It can be welded after quenching and tempering. There is no temper brittleness during heat treatment, but the hardenability is low. It is used as small-section quenched and tempered parts that bear large loads or large normalized parts with small stress, as well as surface, quenched parts that do not require high core strength and wear-resistant surfaces, such as crankshafts, spindles, drive shafts, connecting rods, etc. Tie rod, tooth.
S40C
Alloy
S40C is an alloy with high strength, good machinability, medium cold deformation ability, poor weldability, no temper brittleness, low hardenability, and prone to water quenching cracks.
Features and Applications
It is mostly used in the quenched and tempered or normalized state. The comprehensive properties of the two are similar. After surface quenching, it can be used to manufacture parts that can withstand greater stress. It is suitable for manufacturing crankshaft spindles, drive shafts, piston rods, connecting rods, sprockets, gears, etc. It needs to be preheated before welding and slowly cooled after welding.
Mechanical Properties
Tensile strength σb (MPa): ≥570
Yield strength σs (MPa): ≥335
Sectional shrinkage ψ/(%): ≥45
Impact absorption energy (Aku2/J): ≥47
The hardness of steel as delivered: HBS 10/3000: Unheated steel ≤217 Annealed steel ≤187
Recommended heat treatment/°C Normalizing 860 Quenching 840 Tempering 600
Sample size: Sample blank size/mm: 25