Gear Ring PM Sintered Part
Powder metallurgy technology is a net-shaping or near-net-shaping technology. It uses the characteristics of powder to be easy to shape. It not only has high product precision, but also has a high material utilization rate. It is an efficient and environmentally friendly technology, especially for workpieces with complex shapes.
Product Introduction
|
Gear ring PM sintered part |
||||||
|
Item |
Material |
Production Process |
Sintering Temperature |
Mold |
Custom |
|
|
Gear ring powder metallurgy |
40rc |
Powder metallurgy |
1180℃ |
To be customized |
Yes |
|
|
Chemical composition |
C:0.37~0.44 Si:0.17~0.37 Mn:0.50~0.80 Cr:0.80~1.10 Ni:≤0.30 P:≤0.035 S:≤0.035 Cu:≤0.25 Mo:≤0.10 |
|||||
|
Available Materials |
Low carbon stainless steel, titanium alloy (Ti, TC4), copper alloy, tungsten alloy, hard alloy, high temperature alloy (718, 713) |
|||||
Product advantages
|
Smoothness |
Dimensional accuracy |
Product density |
Appearance treatment |
Appropriate weight |
|
Roughness 1~5μm |
(±0.1%~±0.5%) |
92~95% |
According to customer requirements |
0.03g~400g) |
|
mechanical properties |
Sample blank size (mm): 25 heat treatment: Heating temperature for the first quenching (℃): 850; coolant: oil Second quenching heating temperature (°C):- Tempering heating temperature (°C): 520; Tensile strength (σb/MPa): ≥810 (when the actual hardness is 25HRC) Yield point (σs/MPa): ≥785 Elongation after break (δ5/%): ≥9 Reduction of area (ψ/%): ≥45 Impact absorption energy (Aku2/J): ≥47 Brinell hardness (100/3000HBW) (annealed or high temperature tempered state): ≤207 |
|||
Process Flow
The invention belongs to the field of powder metallurgy, in particular to a gear, a gear ring and a method for one-time forming thereof by powder metallurgy.
Background technique:
Powder metallurgy technology is a net-shaping or near-net-shaping technology. It uses the characteristics of powder to be easy to shape. It not only has high product precision, but also has a high material utilization rate. It is an efficient and environmentally friendly technology, especially for workpieces with complex shapes. Machining Difficult to do, but easily achievable with powder metallurgy technology. In addition, the holes left in the sintering process can absorb vibration and reduce noise under the working conditions with lower mechanical performance requirements, and can also play a self-lubricating role for workpieces such as bearings. However, in the working conditions with high requirements on mechanical properties, powder metallurgy products usually require additional processes to improve their mechanical properties, such as surface rolling, infiltration, etc. Too complicated additional process will reduce the competitiveness of powder metallurgy products.
Technical realization elements:
The object of the present invention is to overcome the above-mentioned shortcomings of the prior art, and provide a gear and ring gear and a method for one-time forming thereof by powder metallurgy.
In order to achieve the above object, the present invention adopts the following technical solutions to achieve:
A method for forming a gear and a gear ring at one time by powder metallurgy, comprising the following steps:
1) According to the gear shape and mechanical performance requirements, calculate the material size of the area to be forged, and design the cold pressing die;
2) Configure the powder and mix the materials. After the mixing is completed, use a cold-press mold to perform cold-press forming to obtain cold-pressed parts of gears or gear rings;
3) Sintering the cold-pressed part to obtain a sintered part;
4) Inductively heat the sintered part, and when the outer surface of the sintered part reaches 1080-1200°C, transfer it to the hot forging die cavity for hot forging within 2-5s to obtain the intermediate part;
5) Finishing the middleware to obtain the final product.
Further, in step 1), calculate and use finite element simulation software to determine the size of the cold-pressed part, and design the cold-pressed mold.
Further, in step 2), the mixed powder is configured according to the following mass percentages: copper 2.50%, graphite 0.5-0.64%, binder 0.45-0.6%, and the balance is iron; cold pressing is carried out under a pressure of 500-600mpa , to obtain cold-pressed parts with preset shape and density.
Further, in step 2), the mixed powder is configured according to the following mass percentages: 0.5-4% nickel, 0.2-4% molybdenum, 0.5-3.2% copper, 0.5-0.8% graphite, 0.4-0.9% binder, and The amount is iron; cold pressing is performed under a pressure of 500-600mpa to obtain a cold pressed piece with a preset shape and density.
Further, step 3) comprises the following steps:
31) Degrease the pre-pressed parts in an atmosphere of 300-400 ° C and a volume ratio of n2 and h2 with a volume ratio of 9:1 for 10 minutes;
32) Sinter at 1120-1200° C. in an atmosphere of n2 and h2 with a volume ratio of 9:1 for 30-40 minutes to obtain a sintered part.
Further, step 4) comprises the following steps:
41) Put the sintered gear into the semi-closed sleeve, place the semi-closed sleeve in the induction coil, and pass inert gas into the semi-closed sleeve;
42) Turn on the induction coil to start heating the sintered part, until the outer surface of the sintered part reaches 1080-1200°C, stop heating;
43) Transfer the sintered part after induction heating to the hot forging die cavity for hot forging within 2-5s to obtain the intermediate part.
Further, step 5) comprises the following steps:
51) Quenching the uncooled intermediate piece after hot forging;
52) Remove the oxide layer and flash to obtain the final product.
8. A method for forming gears and ring gears by powder metallurgy as claimed in claim 1, wherein step 5) comprises the following steps:
51) Deoxidize and flash the cooled intermediate piece to obtain the final product.
A gear and a ring obtained by the partial forging method of the gear ring described above.
Compared with the prior art, the present invention has the following beneficial effects:
The invention provides a partial forging method of a gear tooth ring, which utilizes powder metallurgy technology for one-time forming, respectively undergoes mold design, cold pressing forming, sintering, induction heating, local hot forging and finishing, and each part of the later stage is molded when designing the cold pressing die. The density of the stage is taken into account, so that the final product made of the pre-pressed part after cold pressing and the subsequent steps meets the size requirements, and the forming is convenient and controllable; the sintered part after induction heating has the highest surface temperature, from the surface to the center The temperature decreases gradually, and when the surface reaches 1080-1200°C, a forgeable area with a certain thickness is formed on the surface, and then an unforgeable area is formed in the middle, which saves energy and is convenient for forging, and overcomes the need to forge directly with sintered parts during the sintering process when the furnace is opened. The problem that the reducing atmosphere is prone to explosion; the present invention provides a gear and ring gear obtained by this method, the strength of the tooth root is improved by local forging, and the core area still maintains the characteristics of powder metallurgy products with pores, so as to prevent To the effect of shock absorption, noise reduction and self-lubrication, the core part is easy to demould during hot forging.
Among them: 1-upper punch; 2-locally reinforced sintered parts; 3-middle mold; 4-lower punch; 5-induction coil; 6-semi-closed quartz tube; volume ratio.
Detailed ways
In order to enable those skilled in the art to better understand the solutions of the present invention, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only It is an embodiment of a part of the present invention, but not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by persons of ordinary skill in the art without making creative efforts shall fall within the protection scope of the present invention.
It should be noted that the terms "first" and "second" in the description and claims of the present invention and the above drawings are used to distinguish similar objects, but not necessarily used to describe a specific sequence or sequence. It is to be understood that the data so used are interchangeable under appropriate circumstances such that the embodiments of the invention described herein can be practiced in sequences other than those illustrated or described herein. Furthermore, the terms "comprising" and "having", as well as any variations thereof, are intended to cover a non-exclusive inclusion, for example, a process, method, system, product or device comprising a sequence of steps or elements is not necessarily limited to the expressly listed instead, may include other steps or elements not explicitly listed or inherent to the process, method, product or apparatus.
The present invention is described in further detail below in conjunction with accompanying drawing:
Example 1
1) Configure the mixed powder according to the following mass percentages: 2.50% copper, 0.64% graphite, 0.45% binder, and the balance is iron; fully mix evenly in the powder mixer; wherein, the binder can be selected from stearic acid, hard One or more of zinc fatty acid, glycerol ethanol solution and paraffin ether solution.
2) Determine the size of the pre-pressed part according to the finite element simulation software, design the cold-pressing mold, and perform cold-pressing under a pressure of 600mpa to obtain a cold-pressed part with a preset shape and density; among them, the factors affecting the size of the pre-pressed part include sintering Changes in density during the process, changes in density during partial forging, and changes in density during cooling.
3) Sinter the cold-pressed part obtained in step 2), first degrease the prefabricated part at 400°C, 90%n210%h2 in a reducing atmosphere for 10 minutes; then degrease at 1180°C, 90%n210%h2 Sintered in a neutral atmosphere for 40 minutes to obtain a sintered part;
4) The sintered part is heated by induction. Specifically, the sintered part is put into a semi-closed quartz tube, an inert gas is passed through the upper end of the quartz tube, and the induction coil is wound outside the quartz tube; the induction coil is energized, and the heating is stopped when the temperature of the outer surface of the sintered part reaches 1080 ° C; The heated sintered parts are transferred to the hot forging die cavity for hot forging within 2 seconds, and air-cooled after forging to obtain intermediate parts.
5) Finishing the intermediate piece to achieve the required precision and smoothness, and then quenching to increase the hardness after secondary heating, so as to obtain the powder forged gear with local high density.
In another embodiment, it is transferred to the hot forging die cavity in step 4), and the temperature of the hot forging die cavity is 300° C.; this embodiment is beneficial to control the temperature during hot forging.
Referring to Fig. 1, Fig. 1 is the cold-pressed part formed through step 1); See Fig. 2, Fig. 2 is the finished product after finishing; In step 4, the sintered part 2 after induction heating is placed in a hot forging die, the sintered part 2 after induction heating is placed in the middle mold 3, and the upper and lower surfaces of the sintered part 2 after induction heating are respectively pressed with upper punches 1 and undershoot 4. From the comparison of Figure 1 and Figure 2, it can be seen that there is a forgeable area on the sintered part. Due to induction heating, the forgeable area is formed from the outer surface to a certain thickness. Putting it into the mold in Figure 3, the forgeable area is obtained by forging the shape Change to a preset shape.
On the other hand, the temperature gradient of the sintered part after induction heating decreases gradually from the surface to the center temperature, so there is no problem of adhesion between the inside of the gear and the mold during hot forging.
Referring to Fig. 6, Fig. 6 is the schematic diagram that the induction coil provided by the present invention is wound on the semi-closed sleeve; during induction heating in step 4), the inert gas is first introduced into the quartz tube, and the sintered part is placed in the quartz tube. By doing so, oxidation and decarburization during heating can be reduced.
One embodiment is to make a semi-closed sleeve with an outer diameter of 20 mm using pvc material, the thickness of the cylinder wall is 2 mm, and it is inserted into an induction coil with an inner diameter of 20 mm; the upper opening of the semi-closed sleeve is fed with inert gas, argon or Nitrogen gas, under the coil is a lifting mechanism, when the workpiece needs to be heated, it rises and enters the gas, and then conducts induction heating. After heating, the lifting mechanism descends, and the workpiece is removed by the manipulator for subsequent operations, such as forging, quenching or welding. In another embodiment, the semi-closed sleeve is made of quartz material.
Example 2
1) Configure the mixed powder according to the mass percentage of the following components: 0.5% nickel, 0.2% molybdenum, 0.5% copper, 0.5% graphite, 0.6% binding agent, and the balance is iron; Mix well and evenly in the powder machine; wherein, the binder can be selected from one or more of stearic acid, zinc stearate, glycerol ethanol solution and paraffin ether solution.
2) Carry out cold pressing according to the size of the pre-pressed part determined by the finite element simulation software, and use the mixed powder obtained in step 1) to carry out cold pressing to obtain a cold-pressed part of the designed size and density;
3) sintering the cold-pressed part obtained in step 2), first degreasing the cold-pressed part at 400°C, 90%n210%h2 in a reducing atmosphere for 10 minutes; then at 1120°C, 90%n210%h2 Sintering in a reducing atmosphere for 40 minutes to obtain a sintered part;
4) The sintered part is heated by induction. Specifically, the sintered part is put into a semi-closed quartz tube, an inert gas is passed through the upper end of the quartz tube, and the induction coil is wound outside the quartz tube; the induction coil is energized, and the heating is stopped when the temperature of the outer surface of the sintered part reaches 1200 ° C; The heated sintered parts are transferred to the hot forging die cavity for hot forging within 5 seconds, and air cooled after forging to obtain intermediate parts.
5) After finishing the intermediate piece to achieve the required precision and smoothness, it is quenched after secondary heating to increase the hardness, so as to obtain the above-mentioned partially high-density powder forged gear ring.
Referring to Fig. 4, Fig. 4 is a drawing of the pre-pressed part of the gear ring provided by the present invention, which is a cold-pressed part of the gear ring after step 2); referring to Fig. 5, Fig. 5 is a finished picture of the gear ring provided by the present invention, which is After steps 3)-5) of the finished gear ring, it can be seen from the comparison of the two figures that after induction heating, a forgeable area is formed from the outer surface to a certain thickness. During the hot forging process, the shape of the forged area is changed after forging. into the default shape.
The specific parameters of other embodiments provided by the present invention are as shown in table 1:
The specific parameters of other embodiments of the present invention in table 1
The above content is only to illustrate the technical idea of the present invention, and cannot limit the protection scope of the present invention. Any changes made on the basis of the technical solution according to the technical idea proposed in the present invention, all fall into the scope of the claims of the present invention. within the scope of protection.
Metal Injection Molding Process