BT6 titanium alloy has natural high strength, low specific gravity and excellent corrosion resistance, so it has been widely and successfully used in aerospace, offshore oil and gas engineering, automobile, chemical industry, medicine and other fields. In many engineering applications, titanium has achieved weight reduction and easy maintenance, thereby improving production benefits.

BT6 Titanium Alloy Introduction
BT6 alloy is the most widely used titanium alloy in the world, with a+ type two-phase structure at room temperature, hence the name a+p type titanium alloy. It has good comprehensive mechanical properties, can be strengthened by heat treatment, has good forging, stamping and welding performance, excellent cutting performance and resistance to hot salt stress corrosion; BT6 titanium alloy also has the characteristics of low density, high specific strength, low elastic modulus, low thermal conductivity, non-magnetic and non-toxic.
Chemical Composition of BT6 Titanium alloy
| Aluminum AL | 5.30-6.80%; |
| Vanadium V | 3.50-5.30% |
| Iron Fe | ≤0.3% |
| Carbon C | ≤0.1%, |
| Nitrogen N | ≤0.05%, |
| Hydrogen H | ≤0.015%, |
| Oxygen 0 | ≤0.20% |
| Titanium Ti | Remainder |
Mechanical Properties of BT6 Titanium alloy
| Tensile strength ob (MPa) | ≥890 |
| Specified residual elongation stress or0.2 (MPa) | 2820 |
| Elongation 65 (%) | 28 |
| Sectional shrinkage y (%) | ≥20 |
| Brinell hardness (HBS10/1500) (annealed state) | ≤350 |
BT6 Titanium Alloy Heat Treatment Process
1. Stress relief annealing: The purpose is to eliminate or reduce the residual stress generated during the processing. Prevent chemical erosion and reduce deformation in some corrosive environments.
2. Complete annealing: The purpose is to obtain good toughness, improve processing performance, facilitate reprocessing and improve the stability of size and structure.
3. Solution treatment and aging: The purpose is to improve its strength. A+P titanium alloy can be further strengthened by solution treatment and aging.
BT6 Titanium Alloy Application Scope
Density [mathematical formula] " [mathematical formula], body, tank tracks, aircraft engine compressor blades, rocket engine casings, liquid hydrogen fuel tank components for rockets and missiles, heaters for petroleum refining and seawater desalination, and environmental pollution control devices, etc.
Characteristics Of Titanium And Titanium Alloys
1: High specific strength.
2: Excellent corrosion resistance.
3: Low elastic modulus.
4: Good heat resistance.
5: Good low temperature performance.
6: High biocompatibility.
7: Low thermal conductivity.
8: Colorful oxide film.
9: Non-magnetic and non-toxic.
10: Strong anti-damping performance.
Application Fields
Due to the excellent properties of titanium and titanium alloys, they are widely used in aerospace, shipbuilding, metallurgy, electronics, chemical industry, petroleum, mechanical equipment, electroplating equipment, sports goods, watches, glasses, jewelry, environmental protection, medical equipment, golf, precision machining, marine engineering, thermal engineering, construction engineering, automobile industry, furniture and daily consumer goods.
Qinhuangdao Zhongwei Precision Machinery Co., Ltd. is a high-tech enterprise specializing in metal powder injection molding (MIM) and R&D, production and service. We have a complete production system of design-mold making-batch-sintering-machining-grinding and polishing-assembly. The company passed ISO9001:2008 quality system certification in 2015 and obtained Qinhuangdao High-tech Enterprise Certificate in 2017. Our company can produce various structural parts, functional parts and appearance parts with complex three-dimensional shapes according to the needs of different customers. Products are widely used in 3C industry, lock industry, watch and jewelry industry, medical equipment industry, home appliance industry, automobile industry, communication product industry, etc. We are based on a team of talents graduated from the Department of Powder Materials, and provide high-quality products to customers in various industries with rigorous and standardized control processes.
Our efficiency: quotation within 24 hours, 10-15 days mold cycle, 5 days proofing cycle, 7 days bulk cargo cycle.
Our technical team: The R&D team headed by Dr. Chen from Beijing University of Science and Technology has maintained a product development success rate of more than 98% for two consecutive years. The company develops more than 400 new products on average each year, which is more than 80% higher than its peers, and has obtained more than 20 patent certificates. We can produce titanium alloy, stainless steel, high temperature alloy, and other MIM parts for you
Our services: Our company has a complete set of production lines including mold manufacturing, batching, sintering, CNC machining, grinding and polishing, assembly, etc.; customer service actively reports production progress to customers every 3 days.
Our quality: 100% of our products have established a complete set of process data to ensure the quality and stability of different batches, and the average yield rate is controlled at more than 98%.
We will give back to our customers for their long-term support and trust with higher quality and better service. We sincerely invite new and old friends from all walks of life to visit us for guidance, deepen understanding, and sincere cooperation!
AП33 Aluminum Alloy Metal Powder Injection Molding M...
Automobile Rearview Mirror Base Metal Injection Mold...
Automobile Eccentric Shaft Metal Injection Molding M...
Automobile Drum Brake Gear Metal Injection Molding M...
AlMg1SiCu1.5 Metal Injection Molding MIM Parts
38 SD7-154 Chainsaws Sprocket Metal Injection Molding
Send Inquiry