18C3 Lost Wax Investment Casting
18C3 lost wax investment casting has high strength and hardenability. The critical hardenable diameter in oil reaches 4 to 22mm, and the critical hardenable diameter in water reaches 11 to 40mm.
Product Introduction
|
18C3 lost wax investment casting |
|||||||
|
Item |
Material |
Production Process |
Sintering Temperature |
Mold |
Custom |
||
|
18C3 lost wax investment casting |
18C3 |
Molten mold casting |
1380℃ |
To be customized |
Yes |
||
|
Chemical composition |
C: 0.18~0.24 Si: 0.17~0.37 Mn: 0.50~0.80 Cr: 0.70~1.00 S: Allowable residual content ≤0.035 P: Allowable residual content ≤0.035 Ni: Allowable residual content ≤0.030 Cu: Allowable residual content ≤0.030 |
||||||
|
Available Materials |
Carbon steel, alloy steel, aluminum alloy, low -carbon stainless steel, titanium alloy (TI, TC4), copper alloy, high temperature alloy (718, 713) |
||||||
|
Smoothness |
Dimensional accuracy |
Product density |
Appearance treatment |
Appropriate weight |
|||
|
Roughness 1~5μm |
(±0.1%~±0.5%) |
7.8g/CM³ |
According to customer requirements |
3g~4kg) |
|||
18c3 an alloy structural steel
18C3 is a kind of alloy structural steel. This steel is mostly used to manufacture carburized parts (oil quenching) that require high core strength, bear surface wear, have a cross-section below 30mm, or have complex shapes and low loads.
Attributes
18C3, alloy structural steel. Unified digital code: A20202
Standard GB/T 3077-1999 GB/T 17107
Application
This kind of steel is mostly used to manufacture carburized parts (oil quenching) that require high core strength, are subject to surface wear, have a cross-section below 30mm, or have complex shapes and low loads, such as machine tool gearbox gears, gear shafts, and cams. , worm, piston pin, claw clutch, etc.; for parts with small heat treatment deformation and high wear resistance, high-frequency surface quenching should be performed after carburization, such as gears, shafts, splined shafts with a module less than 3, etc. This steel can also be used in the quenched and tempered state to manufacture parts that work at high speeds and withstand moderate impact loads. This steel can also be used as low-carbon martensitic quenching steel to further increase the yield strength and Tensile strength (approximately 1.5 to 1.7 times increased).
Features
18C3 lost wax investment casting has high strength and hardenability. The critical hardenable diameter in oil reaches 4 to 22mm, and the critical hardenable diameter in water reaches 11 to 40mm. However, the toughness is poor. This steel still remains when carburized. The grains tend to grow, and direct quenching at low temperatures has a greater impact on the impact toughness, so a second quenching is required after carburizing to improve the toughness of the core of the part without tempering brittleness; steel has high cold strain plasticity and can be wire drawn in a cold state; The machinability is good under high-temperature normalizing or quenching and tempering conditions, but is poor after annealing; the weldability is good, and heat treatment is generally not required after welding, but parts with a thickness greater than 15mm need to be preheated to 100~150°C before welding.
Chemical composition
(mass fraction) (%)
Carbon C: 0.18~0.24
Silicon Si: 0.17~0.37
Manganese Mn: 0.50~0.80
Chromium Cr: 0.70~1.00
Sulfur S: Allowable residual content ≤ 0.035
Phosphorus P: Allowable residual content ≤0.035
Nickel Ni: Allowable residual content ≤0.030
Copper Cu: Allowable residual content ≤0.030
Delivery Status
Delivery with heat treatment (normalizing, annealing, or high-temperature tempering) or without heat treatment, the delivery status should be specified in the contract.
Detection Systems

Copper Silica Sol Investment Casting