A6061 Aluminum Alloy Metal Powder Injection Molding MIM Parts
A6061 Aluminum Alloy Metal Powder Injection Molding MIM Parts
video
A6061 Aluminum Alloy Metal Powder Injection Molding MIM Parts
A6061_aluminum_alloy_metal_powder_injection_molding_MIM_parts_1720142197307_0.jpg_w720
A6061_aluminum_alloy_metal_powder_injection_molding_MIM_parts_1720142209219_0.jpg_w720
A6061_aluminum_alloy_metal_powder_injection_molding_MIM_parts_1720142218707_0.jpg_w720
A6061_aluminum_alloy_metal_powder_injection_molding_MIM_parts_1720142218707_1.jpg_w720
1/2
<< /span>
>

A6061 Aluminum Alloy Metal Powder Injection Molding MIM Parts

Basic Introduction 6061 T6 has high strength, high hardness (up to HB90 degrees or more), good processing effect, and good oxidation effect. No sand holes and good flatness. Improve processing efficiency and reduce material costs. This will be the best choice for low-price, high-quality...

Basic Introduction

6061 T6 has high strength, high hardness (up to HB90 degrees or more), good processing effect, and good oxidation effect. No sand holes and good flatness. Improve processing efficiency and reduce material costs. This will be the best choice for low-price, high-quality materials. The 6061-T6 series is an aluminum, magnesium, and silicon alloy. It is a heat-treated corrosion-resistant alloy. It has good strength and corrosion resistance, and good uniformity.

 

A6061aluminumalloymetalpowderinjectionmoldingMIMparts17201421973071jpgw720

 

Main Uses

6061 T6 has magnesium and silicon as the main alloying elements. It has medium strength, good corrosion resistance, weldability, and good oxidation effect. It is widely used in various industrial structural parts that require a certain strength (85-110 degrees) and high corrosion resistance, such as railway vehicles, furniture machinery parts, precision machining, molds, etc.

 

Material Strength Design Value

Tensile and compressive strength 200N/mm²
Shear strength 115N/mm²
Local bearing strength 305N/mm²

 

Chemical Composition

Cu 0.15-0.4
Si 0.4-0.8
Fe ≤0.7
Mn ≤0.15
Mg 0.8-1.2
Zn 0.25-0.50
Cr 0.04-0.35
Ti ≤0.15

 

They are four-digit aluminum alloys with magnesium and silicon as the main alloying elements and Mg2Si phase as the strengthening phase.
Alloy state
Report
Editor
T6 The state of artificial aging after solution heat treatment. Applicable to products that are no longer cold-worked after solution heat treatment (straightening and leveling can be performed, but it does not affect the mechanical performance limit).

Qinhuangdao

Zhongwei Precision Machinery Co., Ltd. was founded in 1997 and is a manufacturer and technical solution provider focusing on metal powder injection molding (MIM) and investment casting and forging products. The company is located in Qinhuangdao High-tech Zone, with automotive system 16949 certification, a strong R&D team and technical strength, providing customers with fast and effective solutions and stable product supply.

Since its establishment, the company has always adhered to the principle of customer-oriented, quality-first, independent innovation and continuous improvement. Technology-first development policy.

The company's main business is the research and development, design, production and sales of metal product structural parts. The products can be widely used in key application fields such as consumer electronics, medical devices, and automobiles. It has advantages and rich experience in product research and development, mold development, process design, product manufacturing, quality control, etc.

The company has a stable core team, an excellent technical team, and has introduced advanced equipment to form the core competitiveness of MIM products in the industry and become a strategic partner of MIM products for international customers.

 

Send Inquiry

(0/10)

clearall